霍晓迪, 陈兵, 李知勋等. 过孔的不同干法刻蚀工艺对TFT-LCD性能的影响研究[J]. 液晶与显示, 2016,31(1): 58-61
HUO Xiao-di, CHEN Bing, LEE Ji-Hoon etc. Influence of different dry etching process of contact hole on TFT-LCD performance[J]. , 2016,31(1): 58-61
霍晓迪, 陈兵, 李知勋等. 过孔的不同干法刻蚀工艺对TFT-LCD性能的影响研究[J]. 液晶与显示, 2016,31(1): 58-61 DOI: 10.3788/YJYXS20163101.0058.
HUO Xiao-di, CHEN Bing, LEE Ji-Hoon etc. Influence of different dry etching process of contact hole on TFT-LCD performance[J]. , 2016,31(1): 58-61 DOI: 10.3788/YJYXS20163101.0058.
为了改善过孔的干法刻蚀中刻蚀率的不同导致SD线和P-Si接触面积不一致的问题
同时解决ELA工艺导致P-Si表面突起而造成SD与P-Si点状接触的问题
探究了过孔的不同干法刻蚀工艺对TFT-LCD性能的影响
从中找出最佳的过孔干法刻蚀工艺。利用京东方产线设备制备了两种不同的LTPS阵列样品
样品一的过孔工艺采用传统的底部接触方式
样品二采用新的侧面接触方式
样品一和样品二其余的工艺过程一致。实验结果表明:多点的
U-I
曲线由发散变为集聚
电子迁移率有所提高;SEM数据表明采用侧面接触方式能够完全将P-Si刻穿。采用侧面接触方式能够明显的解决干法刻蚀中刻蚀率的不同导致SD线和P-Si接触面积不一致的问题
同时避免了ELA工艺导致P-Si表面突起而造成SD与P-Si点状接触的问题
电学性能有所改善
同时减少了工艺时间
提高了产能。
In order to overcome the inconsistent contact area between SD line and P-Si caused by the difference of etching rate in via hole dry etching technology
as well as to solve the point contact between SD line and P-Si made by P-Si surface convex during the ELA process
we explored the influence of various via hole dry etching technology upon the property of TFT-LCD
so as to find the optimal via hole dry etching technology.Two different samples of LTPS array were prepared by using BOE production line equipment
wherein the sample 1 was prepared by adopting conventional Just Contact Method
while the sample 2 was prepared by adopting a new type of Side Contact Method. Besides the differences of contacting methods
there is no other differences of technological processes during making these two samples.The experimental results show that the multipoint
U-I
curve changes from a divergent curve to a concentration curve
and electron mobility increases in some degree. In addition
the SEM data show that the P-Si can be cut through completely by Side Contact Method. Side Contact Method is able to overcome the inconsistent contact area between SD line and P-Si caused by the difference of etching rate of via hole dry etching technology
as well as to solve the point contact between SD line and P-Si made by P-Si surface convex during the ELA process
so that the TFT-LCD electrical performance can be improved. In addition
the Side Contact Method can reduce the process time
and improve the productivity.
刘永智,杨开愚.液晶显示技术[M].成都:电子科技大学出版社,2000:339-345. LIU Y Z, YANG K Y. A Liquid Crystal Display Technology[M]. Chengdu:University of Electronic Science and Technology of China Press, 2000:339-345. (in Chinese)
王新久.液晶光学和液晶显示[M].北京:科学出版社,2006:313-319. WANG X J. Liquid Crystal Optical and Liquid Crystal Display [M]. Beijing:Science Press, 2006:313-319. (in Chinese)
DONELAN J.综述:低温多晶硅技术[J].现代显示,2010(10):5-7. DONELANJ. Overview:Low-temperature polysilicon[J]. Advanced Display, 2010(10):5-7. (in Chinese)
黄锡珉.显示技术新进展[J].液晶与显示,2000,15(1):1-5. HUANG X M. New development of display technology[J]. Chinese Journal of Liquid Crystals and Displays, 2000, 15(1):1-5. (in Chinese)
邓泽超,马娜,褚立志,等.激光退火能量对非晶Si薄膜晶化的影响[J].河北大学学报:自然科学版,2008,28(6):592-595. DENG Z C, MA N, CHU L Z, et al. Influence of annealed laser energy on crystallization of amorphous Si thin films[J]. Journal of Hebei University:Natural Science Edition, 2008, 28(6):592-595. (in Chinese)
陈少军,李以贵.基于高深宽比Si干法刻蚀参数优化[J].微纳电子技术,2009,46(12):750-754. CHEN S J, LI Y G. Parameter optimization based on high-aspect ratio Si dry etching[J]. Micronanoelectronic Technology, 2009, 46(12):750-754. (in Chinese)